材料
|
速度
m/min
|
端面铣刀每齿直每径进给(毫米)
|
至6mm
|
至12mm
|
至25mm
|
铝/铝合金
|
183-365
|
,0050-,0500
|
,0050-,1015
|
,1015-,2030
|
黄铜/青铜
|
60-107
|
,0125-,0500
|
,0050-,0760
|
,760-,1250
|
铜/铜合金
|
107-275
|
,0125-,0500
|
,0500
|
,0500-,1525
|
软铸铁
|
60-153
|
,0125-,0500
|
,0500-,0760
|
,0760-,2030
|
硬铸铁
|
24-107
|
,0075-,0200
|
,0200-,0500
|
,0500-,1015
|
球墨铸铁
|
24-122
|
,0050-,0250
|
,0250-,0500
|
,0500-,1525
|
锻化铁
|
122183
|
,0050-,0250
|
,0250-,0760
|
,0760-,1780
|
镁/镁合金
|
245427
|
,0125-,0500
|
,0500-,1015
|
,1015-,2540
|
蒙乃尔台金/高镍钢
|
45-90
|
,0500-,0250
|
,0250-,0500
|
,0500-,1015
|
镍基高温合金
|
6-40
|
,0075-,0200
|
,0200-,0250
|
,0250-0500
|
塑料
|
183-365
|
,0150-,0750
|
,0760-,1525
|
,1525-,3800
|
实心有机玻璃
|
90-245
|
,0150-,0750
|
,0760-,1015
|
,1015-,3045
|
耐火台金
|
24-122
|
,0050-,0250
|
,0250
|
,0250-,0500
|
低碳钢
|
60-153
|
,0050-,0250
|
,0250-,0760
|
,0760-,1780
|
中碳钢
|
30-75
|
,0050-,0380
|
,0380-,0500
|
,0500-,1250
|
硬质钢
|
7-37
|
,0050-,0125
|
,0125-,0250
|
,0250-,0760
|
磨具钢
|
60107
|
,0050-,0250
|
,0250-0506
|
,0500-,1525
|
工具钢
|
30-90
|
,0050-,0250
|
,0250-,0500
|
,0506-,1525
|
软不锈钢
|
45-107
|
,0050-,0250
|
,0250-,6500
|
,0500-,1525
|
硬不锈钢
|
15-60
|
,0050-,0125
|
,0125-,0250
|
,0250-,1250
|
软钛
|
35-107
|
,0056-,0250
|
,0250-,6500
|
,0500-,1525
|
硬钛
|
9-45
|
,0050-,0125
|
,0125-,0256
|
,0250-,1015
|
较小的径向切削深度—采用推荐表面速度的高范围值
较大的径向切削深度—采用推荐表面速度的高范围值
铣槽时一最低范围值速度再降约百分之二十
当轴向切削深度不超过工具直径的1-1/2倍时请用上述推荐表
使用长柄或加长柄端面铣刀时降低进给速度每齿50%
所有推荐值仅供启动时考虑,可加调整以达最佳效果。 |